Electrical transport and percolation in magnetoresistive manganite / insulating oxide composites: case of La0.7Ca0.3MnO3 / Mn3O4
Abstract
We report the results of electrical resistivity measurements carried out on well-sintered La0.7Ca0.3MnO3 / Mn3O4 composite samples with almost constant composition of the magnetoresistive manganite phase (La0.7Ca0.3MnO3). A percolation threshold (fc) occurs when the La0.7Ca0.3MnO3 volume fraction is ~ 0.19. The dependence of the electrical resistivity as a function of La0.7Ca0.3MnO3 volume fraction (fLCMO) can be described by percolation-like phenomenological equations. Fitting the conducting regime (fLCMO > fc) by the percolation power law returns a critical exponent t value of 2.0 +/- 0.2 at room temperature and 2.6 +/-0.2 at 5 K. The increase of t is ascribed to the influence of the grain boundaries on the electrical conduction process at low temperature.
- Publication:
-
arXiv e-prints
- Pub Date:
- March 2007
- DOI:
- 10.48550/arXiv.cond-mat/0703367
- arXiv:
- arXiv:cond-mat/0703367
- Bibcode:
- 2007cond.mat..3367V
- Keywords:
-
- Condensed Matter - Materials Science
- E-Print:
- 7 pages, 3 figures, accepted for publication in Phys. Rev. B