Generation of silicone poly-HIPES with controlled pore sizes via reactive emulsion stabilization
Abstract
Macrocellular silicone polymers are obtained after solidification of the continuous phase of a PDMS (polydimethylsiloxane) emulsion, which contains PEG (polyethylene glycol) drops of sub-millimetric dimensions. Coalescence of the liquid template emulsion is prohibited by a reactive blending approach. We investigate in detail the relationship between the interfacial properties and the emulsion stability, and we use micro- and millifluidic techniques to generation macro-cellular polymers with controlled structural properties over a wider range of cell-sizes (0.2-2mm) and volume fractions of the continuous phase (0.1-40%). This approach could easily be transferred to a wide range of polymeric systems.
- Publication:
-
arXiv e-prints
- Pub Date:
- October 2016
- DOI:
- 10.48550/arXiv.1610.06327
- arXiv:
- arXiv:1610.06327
- Bibcode:
- 2016arXiv161006327G
- Keywords:
-
- Condensed Matter - Soft Condensed Matter
- E-Print:
- Macromolecular Rapid Communications 37,18 (2016): 1527-1532