Electronic charges and electric potential at LaAlO3/SrTiO3 interfaces studied by core-level photoemission spectroscopy
Abstract
We studied LaAlO3/SrTiO3 interfaces for varying LaAlO3 thickness by core-level photoemission spectroscopy. In Ti 2p spectra for conducting “n-type” interfaces, Ti3+ signals appeared, which were absent for insulating “p-type” interfaces. The intensity of the Ti3+ signals was significantly higher than that expected for the transport carrier densities, indicating that part of the carriers at the interfaces are localized. The Ti3+ signals increased with LaAlO3 thickness, but started well below the critical thickness of 4 unit cells for metallic transport. Core-level shifts with LaAlO3 thickness were much smaller than predicted by the polar catastrophe model. We attribute these observations to surface defects and/or adsorbates providing charges to the interface even below the critical thickness.
- Publication:
-
Physical Review B
- Pub Date:
- December 2011
- DOI:
- arXiv:
- arXiv:1106.3619
- Bibcode:
- 2011PhRvB..84x5124T
- Keywords:
-
- 73.20.-r;
- 73.40.-c;
- 73.90.+f;
- 79.60.Jv;
- Electron states at surfaces and interfaces;
- Electronic transport in interface structures;
- Other topics in electronic structure and electrical properties of surfaces interfaces thin films and low-dimensional structures;
- Interfaces;
- heterostructures;
- nanostructures;
- Condensed Matter - Materials Science
- E-Print:
- Phys. Rev. B 84, 245124 (2011)