Composition of Copper Tarnish Products Formed in Moist Air with Trace Levels of Pollutant Gas: Hydrogen Sulfide and Sulfur Dioxide/Hydrogen Sulfide
Abstract
- Publication:
-
Journal of the Electrochemical Society
- Pub Date:
- November 1995
- DOI:
- 10.1149/1.2048404
- Bibcode:
- 1995JElS..142.3723R